XRD phase investigations of steam oxidized Fe and Ni rich Cr alloys


The aim of this work was to summarise XRD investigations performed after the tests carried out in steam oxidation conditions in the temperature range 700‒800°C for 3000 hours. In this work, two solid-solution strengthened alloys; Haynes®...

more >>


High temperature corrosion of metallic materials in coal fired power plant boilers


The aim of this work was to perform high temperature tests in steam conditions at 700‒800°C for 3000 hours. In this work seven alloys were studied: Cr rich austenitic steels 309S, 310S, HR3C, and two solid-solution strengthened Ni based allo...

more >>