The aim of this work was to summarise XRD investigations performed after the tests carried out in steam oxidation conditions in the temperature range 700‒800°C for 3000 hours. In this work, two solid-solution strengthened alloys; Haynes...
więcej >>
The aim of this work was to perform high temperature tests in steam conditions at 700‒800°C for 3000 hours. In this work seven alloys were studied: Cr rich austenitic steels 309S, 310S, HR3C, and two solid-solution strengthened Ni based allo...